A-249 Welded – ASTM Specifications

A249 specification covers nominal-wall-thickness welded tubes and heavily cold worked welded tubes made from austenitic steels, with various grades intended for use as boiler, superheater, heat exchanger, or condenser tubes.

  304 304L 316 316L
Carbon, max, % 0.08 0.030 0.08 0.030
Manganese, Max, % 2.00 2.00 2.00 2.00
Phosphorous, Max, % 0.045 0.045 0.045 0.045
Sulfur, Max, % 0.03 0.03 0.03 0.03
Silicon, Max, % 1.00 1.00 1.00 1.00
Chromium, % 18.0 – 20.0 18.0 – 20.0 16.0 – 18.0 16.0 – 18.0
Nickel, % 8.0 – 11.0 8.0 – 12.0 10.0 – 14.0 10.0 – 14.0
Molybdenum, % 0 0 2.00 – 3.00 2.00 – 3.00
  304 304L 316 316L
Tensile Strength Minimum ksi (MPa) 75 (515) 70 (485) 75 (515) 70 (485)
Yield Strength Minimum ksi (MPa) 30 (205) 25 (170) 30 (205) 25 (170)
Elongation Min 35% 35 35% 35
Rockwell Hardness Number, maximum B90 B90 B90 B90
All wall thickness’ +20% / 0%
Outside Diameters Under 1.000″ +0.004″ / -0.004″
Outside Diameters 1.000″ – 1.500″ inclusive +0.006″” / -0.006″
Outside Diameters 1.501″ – 2.000″ +0.008″ / -0.008″
Outside Diameters 2.001″ – 2.500″ +0.010″ / -0.010″
Outside Diameters 2.501″ – 2.999″ +0.012″ / -0.012″
Outside Diameters 3.000″ – 4.000″ +0.015″ / -0.015″